Title: | Synthèse, étude structurale et morphologique des nouveaux matériaux en céramique |
Authors: | KAHOUL Fares LEBSSISSE, Lamia |
Keywords: | Raman DRX PZT synthèse propriétés électromécaniques, propriétés piézoélectrique propriétés diélectriques Raman synthesis PZT piezoelectric properties XRD dielectric properties electromechanical properties |
Issue Date: | 2017 |
Series/Report no.: | 2017; |
Abstract: | Une série de compositions de céramiques piézoélectrique de type PZT de formule
générale Pb
1-x Yx/2
Bix/2
[(Zr
0.53
Ti0.47
)
0.92
– (Mn
1/3
Sb
2/3
)
0.08] O
3
où x = 0.00, 0.01,
0.02, 0.03, 0.04, 0.05 successivement, ont été élaborées par voie solide et à une
température de frittage 1100°C. Plusieurs techniques ont été utilisées pour
caractériser nos produits : la diffraction de rayon X (DRX) et la spectroscopie
Raman. Cette étude nous à permis de dégager un certain nombre de résultats : la
densité est maximale pour un taux de dopage qui corresponde à une valeur de x=2%,
l’ensemble des échantillons sont cristallisés dans une structure tétragonale, cett e
phase tétragonale de cristallisation est confirmé par la spectroscopie Raman.A series of piezoelectric ceramic compositions Pb1-x Yx/2 Bix/2 [(Zr
0.53
Ti0.47
)0.92 –
(Mn
1/3 Sb2/3
)0.08] O
3 where x = 0.00, 0.01, 0.02, 0.03, 0.04, 0.05 successively , were
prepared by solid route and at a temperature of sintering 1100°C. Several techniques were
used to characterize our samples: The X-ray diffraction (XRD) and Raman spectroscopy. A series of piezoelectric ceramic compositions Pb1-x Yx/2 Bix/2 [(Zr0.53 Ti0.47)0.92 – (Mn1/3 Sb2/3)0.08] O3 where x = 0.00, 0.01, 0.02, 0.03, 0.04, 0.05 successively , were prepared by solid route and at a temperature of sintering 1100°C. Several techniques were used to characterize our samples: The X-ray diffraction (XRD) and Raman spectroscopy. This study with allowed us to release a certain number of results: the density is maximum for a rate of doping which corresponds to a value of x=2%, the whole of the samples are crystallized in a structure tetragonal, this phase tetragonal of crystallization is confirmed by the Raman spectroscopy. |
Description: | Génie de l'environnement |
URI: | http://dspace.univ-ouargla.dz/jspui/handle/123456789/15289 |
Appears in Collections: | Département de Génie des procédés - Master |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
LEBSSISSE-Lamia.pdf | 12,47 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.